Febrianto, Fauzi and Lee, Seunghwan and Jang, Jaehyuk and Hidayat, Wahyu and Kwon, Jinheon and Kondo, Tetsuo and Kim, Namhun (2014) Tensile Properties and Dimensional Stability of Wood Flour-Reinforced cis-1,4-Isoprene Rubber Composites. Journal of the Faculty of Agriculture Kyushu University, 59 (2). pp. 333-337. ISSN 0023-6152

[img]
Preview
Text
Wahyu Hidayat-Tensile Properties and Dimensional Stability of Wood Flour-Reinforced cis-1,4-Isoprene Rubber Composites.pdf

Download (597kB) | Preview
Official URL: https://www.lib.kyushu-u.ac.jp/en/publications_kyu...

Abstract

Wood flour (WF)–reinforced cis–1,4–isoprene rubber (CIR) composite was prepared through a melting process. Maleic anhydride (MAH), dicumyl peroxide (DCP), and zinc oxide (ZnO) were added to the composites to enhance their tensile properties and dimensional stability. The dependence of MAH, DCP and ZnO concentration at various pressing time on tensile strength, elongation at break, Young’s modulus, water absorption (WA) and thickness swelling (TS) of WF–CIR composites were examined. The tensile strength, elongation at break, and Young’s modulus of the WF–CIR were greatly influenced by MAH content and pressing time. The higher the MAH cocentration and the longer time were applied, the greater improvement of tensile strength, Young’s modulus, water absorption and thickness swelling parameters were obtained. However, the elongation at break was found to decrease with addition of MAH. DCP and ZnO concentration were also influenced the tensile strength, elongation at break and Young’s modulus for WF–CIR composites.

Item Type: Article
Uncontrolled Keywords: cis–1,4–isoprene rubber, composites, dicumyl peroxide, maleic anhydride, wood flour.
Subjects: S Agriculture > SD Forestry
Divisions: Fakultas Pertanian (FP) > Prodi Kehutanan
Depositing User: Wahyu Hidayat
Date Deposited: 27 Oct 2016 02:33
Last Modified: 27 Oct 2016 02:33
URI: http://repository.lppm.unila.ac.id/id/eprint/944

Actions (login required)

View Item View Item